Its shore hardness is standard for TPU at 95A, which means it really is gentle and flexible similar to a flip-flop or perhaps a tire. Naturally this all depends on how thick you make the walls and infill. Our sample print used 2 partitions and ten% infill, turning the Thwack https://3dprinterfilament59269.nizarblog.com/33274490/top-guidelines-of-esun-abs-filament